D&J Chemicals was founded in 2013, the enterprise is located in Jinzhou Economic Development Zone, Hebei Province. It covers an area of more than 27,000 square meters and has an annual yield of 10,000 tons of methyl cellulose.
Application and problem analysis of hydroxypropyl methylcellulose in putty!
Insufficient cementitious materials, insufficient water retention of cellulose, low calcium content of heavy calcium, and construction performance: improved by bentonite and starch ether, resulting in hollowing; Insufficient adhesion to the wall, layering: interface treatment, strength: can also be achieved through calcium powder neutral putty:
Powder removal: insufficient cementitious materials, insufficient water retention of cellulose, and low calcium content of heavy calcium
Construction performance: improved through bentonite and starch ether
Empty drum; Insufficient adhesion to the wall caused
Layering: interface processing
Strength: can also be adjusted through calcium powder grading
Grey calcium based putty:
The problems that occur include hollowing, yellowing due to powder removal, poor construction performance, powder removal, layering, cracking, and post thickening
Powder removal: insufficient cementitious materials, insufficient or insufficient cellulose water retention, impure gray calcium
Poor construction performance: improved through bentonite and starch ether
Empty drum; Insufficient adhesion to the wall results in appropriate addition of latex powder
Layering: interface processing
Yellowing: Improper selection of cellulose
Cracking: Cracking of the base layer or excessive strength, hard cracking, and excessive coating thickness
Post thickening: Due to different water absorption rates of heavy calcium, it is recommended to choose heavy calcium powder with zero water absorption or extremely low water absorption; Gray calcium contains undigested GaO.
Cement based putty:
The problems include hollowing, poor construction performance, powder peeling, layering, cracking, insufficient water resistance, and false setting
Powder removal: insufficient cementitious material, insufficient cellulose water retention, or insufficient addition amount
Poor construction performance: improved through bentonite and starch ether
Empty drum; Insufficient adhesion to the wall, resulting in reasonable addition of latex powder
Layering: interface processing
Yellowing: Improper selection of cellulose
Insufficient water resistance: insufficient latex powder and insufficient cementitious materials
Cracking: Cracking of the base layer or excessive strength, hard cracking, coating too thick, filling holes with putty
False coagulation: Sodium gluconate can be added to extend the operational time and adjust the grading